Abstract
Point defects, which cause small current increases and increased chip background currents at elevated temperatures can mask potentially early failures. The difficulty of screening point defects will likely also occur in denser geometries. Delta Iddq is shown to help distinguish between early fail and reliable chips at these elevated temperatures. Memory application demonstrates that a variety of delta Iddq tests can screen early fail defects.